 Figure S2.2. The results of scanning electron microscopy (SEM) in conjunction with the associated energy-dispersive X-ray spectroscopy (EDX) analysis from (a) Ag 500 , (b) Ni 500, and (c) Zn 500 electrodes after 5 hrs of CO2 electrolysis. Ag OTf was used as reference solution. a b c