Figure S3.2. Comparisons of the stable electrochemical activity of MM and t-Bu for CO2 reduction. The charges transferred in the presence of 0.5 molar % of MM NTf2 and 0.5 molar % of t-Bu NTf2. The potential was constant at -1.8 V vs. Ag/Ag+, and the reactor was purged with 5 mL/min CO2. The stability of t-Bu NTf2 was also checked after chronoamperometry (Figures S3.34 to S3.36).